Polymer Property : Puncture Energy = 3.16 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 4.28 J
3.16 ft-lb
Dow Method
Dow AFFINITY™ PL 1850G Polyolefin Plastomer (POP)
AFFINITY™ PL 1840G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed to provide blown and cast film products with low temperature sealability, excellent optics and g..