Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 38.0 - 55.0 J @Temperature -40.0 - -40.0 °C |
28.0 - 40.6 ft-lb @Temperature -40.0 - -40.0 °F |
Average value: 47.7 J Grade Count:12 |
Overview of materials for PCTG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Puncture Energy | 38.0 - 40.0 J | 28.0 - 29.5 ft-lb | Average value: 39.5 J Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |
|||
Puncture Energy | 38.0 J | 28.0 ft-lb | Puncture energy +23°C |
Ineos ABS Triax® 1120 ABS + Polyamide Blend (Conditioned) Key Features:UnfilledPlatableHigh impact or high impact modifiedSuitable processing methods:Injection moldingFilm extrusionBlow molding |
|||
Puncture Energy | 38.0 J | 28.0 ft-lb | Puncture energy +23°C |
Ineos ABS Triax® KU 2-3050 ABS + Polyamide Blend (Conditioned) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightHeat stabilized or stable to heatSuitable processing methods:Injection molding |
|||
Puncture Energy | 38.0 J @Temperature -40.0 °C |
28.0 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ASTM D3763 |
Eastman DuraStar DS1900HF Polymer, Natural Durastar DS1900HF polymer is a high flow grade of Durastar . Durastar DS1900HF flow lengths are increased 20-40% relative to Durastar DS1000 as shown by spiral flow testing. Other outstanding featur.. |
|||
Puncture Energy | 38.0 J @Temperature -40.0 °C |
28.0 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ASTM D3763 |
Eastman DuraStar DS1910HF Polymer, Natural Durastar DS1910HF polymer is a high flow grade of Durastar that contains a mold release. Durastar DS1910HF flow lengths are increased 20-40% relative to Durastar DS1010 as shown by spiral flow testi.. |
|||
Puncture Energy | 38.0 J @Temperature -40.0 °C |
28.0 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ASTM D3763 |
Eastman DuraStar MN630 Polymer, Natural Durastar Polymer MN630 has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. MN630 has very .. |
|||
Puncture Energy | 38.0 J @Temperature -40.0 °C |
28.0 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ASTM D3763 |
Eastman DuraStar MN631 Polymer, Natural Durastar Polymer MN631 contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing char.. |
|||
Puncture Energy | 38.0 J @Temperature -40.0 °C |
28.0 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ASTM D3763 |
Eastman Eastar AN011 Copolyester Eastar AN011 copolyester is a high flow product. Eastar AN011 flow lengths are increased 20-40% relative to Eastar AN001 as shown by spiral flow testing. Other outstanding features of Eastar are eas.. |
|||
Puncture Energy | 38.0 J @Temperature -40.0 °C |
28.0 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ASTM D3763 |
Eastman Eastar AN014 Copolyester Eastar AN014 copolyester is a high flow product that contains a mold release. Eastar AN014 flow lengths are increased 20-40% relative to Eastar AN004 as shown by spiral flow testing. Other outstandi.. |
|||
Puncture Energy | 38.0 J @Temperature -40.0 °C |
28.0 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ASTM D3763 |
Eastman Eastar MN058 Copolyester Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN058 Copolyester is a medical gra.. |
|||
Puncture Energy | 38.0 J @Temperature -40.0 °C |
28.0 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ASTM D3763 |
Eastman Eastar MN059 Copolyester Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN059 Copolyester is a medical gra.. |