Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 30.0 J | 22.1 ft-lb | ISO 6603-2 |
Lanxess Durethan® A 30 S 000000 Nylon 66 PA 66 standard injection molding-grade, non-reinforced, good demolding, very rapid solidificationApplication Examples: plug connectors, terminal blocks, cable clips, bobbins |
|||
Puncture Energy | 30.0 J | 22.1 ft-lb | Conditioned; ISO 6603-2 |
Lanxess Durethan® BC 40 SR2 000000 Nylon 6 PA 6 injection molding grade, high viscosity, non-reinforced, higher notched impact strength than BC 30, impact-modified |
|||
Puncture Energy | 30.0 J | 22.1 ft-lb | ISO 6603-2 |
Covestro Makrolon® SF805 Polycarbonate, 5% Glass Filled MVR (300 °C/1.2 kg) 7.0 cm3/10 minStructural foam5 % Glass fiber reinforcedNormal fiberChlorine- and bromine-free flame retardantHigh viscosityEasy releaseInjection moldingAvailable in natural (opa.. |
|||
Puncture Energy | 30.0 J @Temperature -30.0 °C |
22.1 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Makrolon® SF800Z Polycarbonate, 5% Glass Filled MVR (300 °C/1.2 kg) 8.0 cm3/10 minStructural foam5 % Glass fiber reinforcedMilled fiberChlorine- and bromine-free flame retardantMedium viscosityEasy releaseInjection moldingAvailable in natural (o.. |