Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 2.00 - 32.0 J @Temperature -30.0 - -30.0 °C |
1.48 - 23.6 ft-lb @Temperature -22.0 - -22.0 °F |
Average value: 15.5 J Grade Count:6 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Puncture Energy | 2.00 - 32.0 J @Temperature -30.0 - -30.0 °C |
1.48 - 23.6 ft-lb @Temperature -22.0 - -22.0 °F |
Average value: 17.6 J Grade Count:5 |
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an.. |
|||
Puncture Energy | 2.00 - 2.00 J @Temperature -30.0 - -30.0 °C |
1.48 - 1.48 ft-lb @Temperature -22.0 - -22.0 °F |
Average value: 2.00 J Grade Count:1 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |
|||
Puncture Energy | 2.00 J @Temperature -30.0 °C |
1.48 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® AKV 30 GIT H2.0 900116 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, suitable for GIT (gas assisted technology), good surface finish, good heat-ageing resistance |
|||
Puncture Energy | 2.00 J @Temperature -30.0 °C |
1.48 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® AKV 30 GIT H2.0 900116 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, suitable for GIT (gas assisted technology), good surface finish, good heat-ageing resistance |
|||
Puncture Energy | 2.00 J | 1.48 ft-lb | ISO 6603-2 |
Lanxess Durethan® BG 30 X 000000 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers/glass spheres, good surface, low warpage |
|||
Puncture Energy | 2.00 J @Temperature -30.0 °C |
1.48 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Durethan® BG 30 X H2.0 901510 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers/glass spheres, good surface, good heat-ageing resistance |
|||
Puncture Energy | 2.00 J @Temperature -30.0 °C |
1.48 ft-lb @Temperature -22.0 °F |
Conditioned; ISO 6603-2 |
Lanxess Durethan® BG 30 X H2.0 901510 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers/glass spheres, good surface, good heat-ageing resistance |
|||
Puncture Energy | 2.00 J | 1.48 ft-lb | ISO 6603-2 |
Lanxess Durethan® BKV 15 G H2.0 900051 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, better surface resistance to alcoholic calcium chloride-solution than BKV 15 H2.0, good heat-ageing resistance |
|||
Puncture Energy | 2.00 J @Temperature -30.0 °C |
1.48 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Lanxess Pocan® DP 1105 000000 PBT PBT, non-reinforced, injection molding, extrusion, improved flowability |
|||
Puncture Energy | 2.00 J | 1.48 ft-lb | 53 N; 40µm sample; ASTM D5748 |
Borealis FA5223 Low Density Polyethylene FA5223 is a Low Density Polyethylene for Film Extrusion. Contains antioxidant and antiblock additive. This grade is developed to give strong film for medium duty applications. Applications FA5223.. |
|||
Puncture Energy | 2.00 J | 1.48 ft-lb | 53 N; 40µm sample; ASTM D5748 |
Borealis FA5224 Low Density Polyethylene FA5224 is a Low Density Polyethylene for Film Extrusion. Contains Antioxidant, Anti-block and Medium Slip additives. This grade is developed to give strong film for medium duty applications. Appl.. |