Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 1.01 J | 0.742 ft-lb | ExxonMobil Method |
ExxonMobil LDPE LD 302.32 Low Density Polyethylene Resin Product Description: LD 302 resins are 3.5% vinyl acetate copolymer, high film resins. The combination of comonomer content and low melt index helps produce films which exhibit superior impact stren.. |
|||
Puncture Energy | 1.01 J | 0.742 ft-lb | ExxonMobil Method |
ExxonMobil LDPE LD 302.56 Low Density Polyethylene Resin Product Description: LD 302 resins are 3.5% vinyl acetate copolymer, high film resins. The combination of comonomer content and low melt index helps produce films which exhibit superior impact stren.. |