Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 55.0 - 75.0 J @Temperature -30.0 - -30.0 °C |
40.6 - 55.3 ft-lb @Temperature -22.0 - -22.0 °F |
Average value: 66.4 J Grade Count:14 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |