Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 2.00 - 2.00 J @Temperature -30.0 - -30.0 °C |
1.48 - 1.48 ft-lb @Temperature -22.0 - -22.0 °F |
Average value: 2.00 J Grade Count:1 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |