Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 45.0 - 60.0 J | 33.2 - 44.3 ft-lb | Average value: 54.0 J Grade Count:5 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Puncture Energy | 45.0 - 47.0 J | 33.2 - 34.7 ft-lb | Average value: 46.3 J Grade Count:8 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Puncture Energy | 45.0 - 45.0 J @Temperature -30.0 - -30.0 °C |
33.2 - 33.2 ft-lb @Temperature -22.0 - -22.0 °F |
Average value: 45.0 J Grade Count:1 |
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Puncture Energy | 45.0 J | 33.2 ft-lb | ISO 6603-2 |
Lanxess Pocan® B 1305 000000 PBT PBT, non-reinforced, injection molding |
|||
Puncture Energy | 45.0 J | 33.2 ft-lb | Puncture Resistance @Max Load, 23°C; ASTM D3763 |
Eastman DuraStar DS2000 Polymer, Natural Durastar DS2000 polymer has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. DS2000 has ver.. |
|||
Puncture Energy | 45.0 J | 33.2 ft-lb | Puncture Resistance @Max Load, 23°C; ASTM D3763 |
Eastman DuraStar DS2110UVI Polymer, Natural Durastar DS2110UVI polymer, contains an ultraviolet light stabilization package. It is recommended for indoor applications requiring enhanced color stability upon extended exposure to fluorescent li.. |
|||
Puncture Energy | 45.0 J | 33.2 ft-lb | Puncture Resistance @Max Load, 23°C; ASTM D3763 |
Eastman DuraStar MN621 Polymer, Natural Durastar Polymer MN621 was developed for the medical device industry and contains a mold release It processes easily and requires minimal drying time. It has superior toughness, high clarity and goo.. |
|||
Puncture Energy | 45.0 J | 33.2 ft-lb | Puncture Resistance @Max Load, 23°C; ASTM D3763 |
Eastman Eastar BR203 Copolyester Eastar BR203 Copolyester contains a mold release additive. It has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilitie.. |
|||
Puncture Energy | 45.0 J @Thickness 3.20 mm |
33.2 ft-lb @Thickness 0.126 in |
At Max load; ASTM D3763 |
Eastman Eastar DN114 Copolyester, Natural Applications:LightingProduct Description: Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage. DN1.. |
|||
Puncture Energy | 45.0 J @Temperature -40.0 °C |
33.2 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ASTM D3763 |
Eastman Eastar EN076 Copolyester Eastar Copolyester EN076 is recommended for the thick-walled containers that are prevalent in the cosmetics and personal care markets. This copolyester offers good processability with the benefits o.. |
|||
Puncture Energy | 45.0 J | 33.2 ft-lb | ISO 6603-2 |
Covestro Makroblend® DP UT3907 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendhigh flowimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT3907* offers superior flowability, good impact strength and excellent ch.. |
|||
Puncture Energy | 45.0 J @Temperature 23.0 °C |
33.2 ft-lb @Temperature 73.4 °F |
ISO 6603-2 |
Covestro Makrolon® 6165 X Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Low.. |
|||
Puncture Energy | 45.0 J | 33.2 ft-lb | ISO 6603-2 |
Covestro Makroblend® DP UT3905 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendhigh flowimpact modifiedeasy releaseinjection molding grade Makroblend DP UT3905* offers superior flowability, good impact strength and excellent chemical resist.. |