Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Unnotched | 48.8 J | 36.0 ft-lb | |
Pacific Sintered Materials FN-262-T High Strength Nickel Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability.Equivalent MPIF Specification: FN-0405-45All information provided by Pacific Sintered Metals. |
|||
Charpy Impact, Unnotched | 48.8 J | 36.0 ft-lb | |
PSM Industries Pacific Sintered Metals High Strength Nickel Steel FN-262-T Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability Equivalent MPIF Specification: FN-0405-45Information Provided by Pacific Sintered Metals, a division.. |