Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Unnotched | 6.78 J | 5.00 ft-lb | |
Pacific Sintered Materials F-240-S Steel Powdered Metal Applications:Medium stressed mechanical componentsEquivalent MPIF Specification: F-0005-25All information provided by Pacific Sintered Metals. |
|||
Charpy Impact, Unnotched | 6.78 J | 5.00 ft-lb | |
Pacific Sintered Materials F-244-S High Carbon Steel Powdered Metal Applications:Highly stressed mechanical componentsGood hardenabilityEquivalent MPIF Specification: F-0008-35All information provided by Pacific Sintered Metals. |
|||
Charpy Impact, Unnotched | 6.78 J | 5.00 ft-lb | |
Pacific Sintered Materials F-244-S(HT) High Carbon Steel Powdered Metal Applications:Highly stressed mechanical componentsGood hardenabilityEquivalent MPIF Specification: F-0008-85(HT)All information provided by Pacific Sintered Metals. |
|||
Charpy Impact, Unnotched | 6.78 J | 5.00 ft-lb | |
Pacific Sintered Materials FCC-200-P High Carbon Copper Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI.. |
|||
Charpy Impact, Unnotched | 6.78 J | 5.00 ft-lb | |
Pacific Sintered Materials FCC-214-S(HT) High Carbon Copper Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPI.. |
|||
Charpy Impact, Unnotched | 6.78 J | 5.00 ft-lb | |
PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-200-P Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MP.. |
|||
Charpy Impact, Unnotched | 6.78 J | 5.00 ft-lb | |
PSM Industries Pacific Sintered Metals High Carbon Steel F-244-S Powdered Metal Highly stressed mechanical components, Good hardenability Equivalent MPIF Specification: F-0008-35Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Charpy Impact, Unnotched | 6.78 J | 5.00 ft-lb | |
PSM Industries Pacific Sintered Metals High Carbon Steel F-244-S(HT) Powdered Metal Highly stressed mechanical components, Good hardenability Equivalent MPIF Specification: F-0008-85(HT)Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Charpy Impact, Unnotched | 6.78 J | 5.00 ft-lb | |
PSM Industries Pacific Sintered Metals Steel F-240-S Powdered Metal Medium stressed mechanical components Equivalent MPIF Specification: F-0005-25Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Charpy Impact, Unnotched | 6.78 J | 5.00 ft-lb | |
PSM Industries Pacific Sintered Metals Bronze BT-126 Powdered Metal Higher strength structural and bearing bronzeInformation Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Charpy Impact, Unnotched | 6.78 J | 5.00 ft-lb | |
PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-214-S(HT) Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MP.. |
|||
Charpy Impact, Unnotched | 6.78 J | 5.00 ft-lb | |
Pacific Sintered Materials BT-126 Bronze Powdered Metal Applications: Higher strength structural and bearing bronze.All information provided by Pacific Sintered Metals. |