Mechanical Properties Metric English Comments
Charpy Impact, Unnotched 48.8 J
36.0 ft-lb
Pacific Sintered Materials FN-262-T High Strength Nickel Steel Powdered Metal
High strength, good impact resistant material for mechanical components. Excellent hardenability.Equivalent MPIF Specification: FN-0405-45All information provided by Pacific Sintered Metals.
Charpy Impact, Unnotched 48.8 J
36.0 ft-lb
PSM Industries Pacific Sintered Metals High Strength Nickel Steel FN-262-T Powdered Metal
High strength, Good impact resistant material for mechanical components, Excellent hardenability Equivalent MPIF Specification: FN-0405-45Information Provided by Pacific Sintered Metals, a division..