Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Unnotched | 176 J | 130 ft-lb | |
PSM Industries PolyAlloys MIM-2700 sintered Low Alloy Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Charpy Impact, Unnotched | 176 J | 130 ft-lb | 1/2 size bar |
Kinetics MIM F75 (ASTM F75) HIP Most commonly used within the medical market on applications requiring these characteristics: Bio-compatibility Corrosion resistance High strength Nonmagnetic Wear resistance. Information prov.. |