Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.40 - 9.32 GPa | 493 - 1350 ksi | Average value: 6.32 GPa Grade Count:16 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |