| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 5.49 GPa | 797 ksi | DIN 53452; ASTM D790 |
| Kolon SPESIN® KP212G15VO G/F Reinforced & Retardant PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
| Flexural Modulus | 5.49 GPa | 797 ksi | DIN 53452; ASTM D790 |
| Kolon SPESIN® KP2122G15VO G/F Reinforced & Retardant PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
| Flexural Modulus | 5.49 GPa | 797 ksi | ASTM D790 |
| Kolon Kocetal® CL704 Reinforced Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
| Flexural Modulus | 5.49 GPa | 796 ksi | ASTM D 790 |
| SABIC Innovative Plastics Lexan® SP7604 PC (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
| Flexural Modulus | 5.49 GPa @Thickness 6.40 mm |
797 ksi @Thickness 0.252 in |
30mm/min; ASTM D790 |
| LG Chemical LUPOL HM2300 PP+GF30% Description: Injection Molding, PP+GF30%, Good WeatherabilityApplication: Electrical, Electronic and Automotive Parts CAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical |
|||
| Flexural Modulus | 5.49 GPa @Thickness 6.40 mm |
797 ksi @Thickness 0.252 in |
1.3mm/min; ASTM D790 |
| LG Chemical LUPOL LW4302 PP+GF/MF30% Description: Injection Molding, PP+GF/MF30%, Low WarpageApplication: Electrical, Electronic and Automotive Parts CAS: 9003-07-0, 14807-96-6 and 165997-17-3Information provided by LG Chemical |
|||
| Flexural Modulus | 5.49 GPa | 796 ksi | 2 mm/min; ISO 178 |
| SABIC Innovative Plastics Valox® SHF434HR PBT PBT, Super High Flow, 20% glass reinforced,hydrolytically resistant. |
|||
| Flexural Modulus | 5.49 GPa | 797 ksi | 2.8 mm/min; ASTM D790 |
| Samsung Cheil Industries Infino® CF-3200HF PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
| Flexural Modulus | 5.49 GPa | 797 ksi | 2.8 mm/min; ASTM D790 |
| Samsung Cheil Industries Infino® EM-8250G MPPE, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
| Flexural Modulus | 5.49 GPa | 796 ksi | ASTM D790 |
| SABIC Innovative Plastics LNP THERMOCOMP Lexan_SP7604 PC (Asia Pacific) |
|||
| Flexural Modulus | 5.49 GPa | 796 ksi | ISO 178 |
| SABIC Innovative Plastics LNP Thermocomp MH0500A PP (Asia Pacific) LNP THERMOCOMP* MH0500A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
| Flexural Modulus | 5.49 GPa | 797 ksi | 2.8 mm/min; ASTM D638 |
| Samsung Cheil Industries Starex® VB-4921 ABS, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
| Flexural Modulus | 5.49 GPa | 797 ksi | 2.8 mm/min; ASTM D790 |
| Samsung Cheil Industries Infino® CF-3200HF PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
| Flexural Modulus | 5.49 GPa | 797 ksi | 2.8 mm/min; ASTM D790 |
| Samsung Cheil Industries Infino® EM-8250G MPPE, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
| Flexural Modulus | 5.49 GPa | 797 ksi | 2.8 mm/min; ASTM D638 |
| Samsung Cheil Industries Starex® VB-4921 ABS, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
| Flexural Modulus | 5.49 GPa | 797 ksi | ASTM D790 |
| Shinkong Synthetic Fibers Shinite® E202G15 PBT, 15% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
| Flexural Modulus | 5.49 GPa | 797 ksi | ASTM D790 |
| Shinkong Synthetic Fibers Shinite® E202G15 PBT, 15% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
| Flexural Modulus | 5.49 GPa @Thickness 6.40 mm |
797 ksi @Thickness 0.252 in |
1.3mm/min; ASTM D790 |
| LG Chemical LUPOL GP2300 PP+GF30% Description: Injection Molding, PP+GF30%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical |
|||