| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 2.61 GPa | 378 ksi | ASTM D790 |
| Techmer ES Plastiblend® POM CO UV BK Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: CopolymerAppearance: BlackInformation provided by TP Composites, Inc. |
|||