| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 2.61 GPa | 379 ksi | ASTM D790 |
| PolyOne Geon™ Vinyl Packaging 2210 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
| Flexural Modulus | 2.61 GPa | 379 ksi | ASTM D790 |
| Network Polymers Kepital® F20-03 Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc. |
|||
| Flexural Modulus | 2.61 GPa | 379 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| SABIC Innovative Plastics Cycoloy® CE3510 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact, high heat and excellent extrusion and thermoforming characteristics. Halogen free.. |
|||
| Flexural Modulus | 2.61 GPa | 379 ksi | Molded; ASTM D790 |
| Honeywell Aegisâ„¢ H135ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon.. |
|||
| Flexural Modulus | 2.61 GPa | 379 ksi | Molded; ASTM D790 |
| Honeywell Aegisâ„¢ H155MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H155MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR.. |
|||
| Flexural Modulus | 2.61 GPa | 379 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| SABIC Innovative Plastics LNP LUBRICOMP IBP34 PA6.12 LNP* LUBRICOMP* IBP34 is a compound based on Nylon 6/12 containing 20% Glass Bead, 15% PTFE/Silicone. Added features include: Wear Resistant. |
|||
| Flexural Modulus | 2.61 GPa | 379 ksi | ASTM D790 |
| Techmer ES Electrablend® PC 04003 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by.. |
|||
| Flexural Modulus | 2.61 GPa | 379 ksi | ASTM D790 |
| Techmer ES Electrablend® PC 04004 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by.. |
|||
| Flexural Modulus | 2.61 GPa | 379 ksi | ASTM D790 |
| Techmer ES Electrablend® PC 04005 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by.. |
|||
| Flexural Modulus | 2.61 GPa | 379 ksi | ISO 178 |
| SABIC Innovative Plastics LNP STAT-KON DD0009PC PC (Asia Pacific) LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
| Flexural Modulus | 2.61 GPa | 378 ksi | ASTM D790 |
| Techmer ES Plastiblend® POM CO UV BK Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: CopolymerAppearance: BlackInformation provided by TP Composites, Inc. |
|||
| Flexural Modulus | 2.61 GPa | 379 ksi | 2 mm/min; ISO 178 |
| SABIC Innovative Plastics NORYL NH5120 PPE+PS Noryl* NH5120 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated V1 flame re.. |
|||
| Flexural Modulus | 2.61 GPa | 379 ksi | ASTM D-790 |
| Axiall 8266 Natural 02 Rigid PVC, Extrusion, Natural 02 Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||