Polymer Property : Flexural Modulus = 0.931 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Modulus 0.317 - 0.931 GPa
46.0 - 135 ksi
Average value: 0.630 GPa Grade Count:67
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Rotational Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Rotational Molded". Each property range of values reported i..