| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 0.317 GPa | 46.0 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
|
Eastman M3019-P Polyethylene
(discontinued **)
M3019-P is suggested for applications such as spiral-wound can linings, release paper, and photographic paper. M3019-P Has been found to exhibit good barrier properties, temperature resistance, and..
|
|||
| Flexural Modulus | 0.317 GPa | 46.0 ksi | at 1% secant modulus; ASTM D790 |
|
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact streng..
|
|||
| Flexural Modulus | 0.317 GPa | 46.0 ksi | at 1% secant modulus; ASTM D790 |
|
A. Schulman CP814-01 Linear, Low-Density Polyethylene
DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA ..
|
|||
| Flexural Modulus |
0.317
GPa <br>@Temperature -20.0 °C
|
46.0
ksi <br>@Temperature -4.00 °F
|
ASTM D790 |
|
DuPont Elvax® 660 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
|
|||
| Flexural Modulus | 0.317 GPa | 46.0 ksi | at 1% secant modulus; ASTM D790 |
|
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact streng..
|
|||
| Flexural Modulus | 0.317 GPa | 46.0 ksi | at 1% secant modulus; ASTM D790 |
|
A. Schulman CP814-01 Linear, Low-Density Polyethylene
DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA ..
|
|||
| Flexural Modulus | 0.317 GPa | 46.0 ksi | at 1% secant modulus; ASTM D790 |
|
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact streng..
|
|||
| Flexural Modulus | 0.317 GPa | 46.0 ksi | at 1% secant modulus; ASTM D790 |
|
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact streng..
|
|||
| Flexural Modulus | 0.317 GPa | 46.0 ksi | at 1% secant modulus; ASTM D790 |
|
A. Schulman CP814-01 Linear, Low-Density Polyethylene
DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA ..
|
|||
| Flexural Modulus | 0.317 GPa | 46.0 ksi | at 1% secant modulus; ASTM D790 |
|
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact streng..
|
|||
| Flexural Modulus | 0.317 GPa | 46.0 ksi | at 1% secant modulus; ASTM D790 |
|
A. Schulman CP814-01 Linear, Low-Density Polyethylene
DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA ..
|
|||
| Flexural Modulus | 0.317 GPa | 46.0 ksi | ASTM D790 |
|
Lubrizol Estane® ALR E65D Thermoplastic Polyurethane
Type: Estane® ALR E65D is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corpor..
|
|||
| Flexural Modulus | 0.317 GPa | 46.0 ksi | at 1% secant modulus; ASTM D790 |
|
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact streng..
|
|||
| Flexural Modulus | 0.317 GPa | 46.0 ksi | at 1% secant modulus; ASTM D790 |
|
A. Schulman CP814-01 Linear, Low-Density Polyethylene
DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA ..
|
|||
| Flexural Modulus | 0.317 GPa | 46.0 ksi | at 1% secant modulus; ASTM D790 |
|
A. Schulman CP814-01 Linear, Low-Density Polyethylene
DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA ..
|
|||
| Flexural Modulus | 0.317 GPa | 46.0 ksi | |
|
Dow DOWLEX™ 2517 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2517 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and low temperature properties with excellent f..
|
|||
| Flexural Modulus | 0.317 - 0.931 GPa | 46.0 - 135 ksi | Average value: 0.630 GPa Grade Count:67 |
|
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Rotational Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Rotational Molded". Each property range of values reported i..
|
|||