Polymer Property : Flexural Modulus = 991 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.600 - 6.83 GPa

@Temperature 100 - 175 °C
87.0 - 991 ksi

@Temperature 212 - 347 °F
Average value: 2.98 GPa Grade Count:4
Overview of materials for Polyphthalamide (PPA), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o..