Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.00 - 5.00 GPa | 580 - 725 ksi | Transverse |
Quadrant Plastic Composites MultiQ® Concrete Thermoplastic Panel Composite MultiQ is a product line of thermoplastic composites in panel form whose specific properties make them particularly suitable as an environmental alternative to plywood in outdoor applications. Howev.. |
|||
Flexural Modulus | 3.50 - 5.00 GPa @Temperature 60.0 - 120 °C |
508 - 725 ksi @Temperature 140 - 248 °F |
Average value: 4.03 GPa Grade Count:2 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Flexural Modulus | 4.00 - 5.00 GPa | 580 - 725 ksi | ASTM D790 |
Chang Chun Plastic PBT3015 15% Glass Fiber Enforced PBT Information provided by Dowell Trading Company Ltd. |
|||
Flexural Modulus | 2.50 - 5.00 GPa @Temperature 60.0 - 120 °C |
363 - 725 ksi @Temperature 140 - 248 °F |
Average value: 3.67 GPa Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |