Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.228 - 3.96 GPa | 33.0 - 575 ksi | Average value: 2.29 GPa Grade Count:106 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |