Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.60 - 35.0 GPa | 957 - 5080 ksi | Average value: 18.0 GPa Grade Count:54 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |