Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.97 - 2.97 GPa @Temperature 120 - 120 °C |
431 - 431 ksi @Temperature 248 - 248 °F |
Average value: 2.97 GPa Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |