Polymer Property : Flexural Modulus = 3250 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.530 - 22.4 GPa
76.9 - 3250 ksi
Average value: 7.86 GPa Grade Count:164
Overview of materials for Nylon 610
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Flexural Modulus 5.52 - 22.4 GPa
800 - 3250 ksi
Average value: 12.9 GPa Grade Count:34
Overview of materials for Nylon 612, Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Carbon Fiber Filler". Each property range of values reported is minimum and maximum values of..