Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.40 - 14.0653 GPa @Temperature -40.0 - 120 °C |
203 - 2040.03 ksi @Temperature -40.0 - 248 °F |
Average value: 6.70 GPa Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |