Polymer Property : Flexural Modulus = 1960 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.758 - 13.5 GPa
110 - 1960 ksi
Average value: 7.83 GPa Grade Count:663
Overview of materials for Nylon 66, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..