Polymer Property : Flexural Modulus = 170 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.772 - 1.17 GPa
112 - 170 ksi
Average value: 0.903 GPa Grade Count:12
Overview of materials for High Density Polyethylene (HDPE), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Impact Grade". Each property range of values reported is minimum and m..