Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.45 - 115 GPa | 210 - 16700 ksi | Average value: 42.4 GPa Grade Count:7 |
Overview of materials for Epoxy Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat.. |