Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.900 - 11.4 GPa | 131 - 1650 ksi | Average value: 3.28 GPa Grade Count:12 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Flexural Modulus | 3.65 - 11.4 GPa | 530 - 1650 ksi | Average value: 9.18 GPa Grade Count:50 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |
|||
Flexural Modulus | 1.88 - 11.4 GPa | 273 - 1650 ksi | Average value: 4.43 GPa Grade Count:104 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |