Polymer Property : Flexural Modulus = 1520 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 6.50 - 10.5 GPa
943 - 1520 ksi
Average value: 8.61 GPa Grade Count:15
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. ..
Flexural Modulus 4.80 - 10.5 GPa
696 - 1520 ksi
Average value: 8.22 GPa Grade Count:21
Overview of materials for Phenolic, Novolac, Mineral/Flock Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Flock Filled". Each property range of values reported is minimum and maximum ..
Flexural Modulus 8.60 - 10.5 GPa
1250 - 1520 ksi
Average value: 9.44 GPa Grade Count:5
Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Cellulose Filled". Each property range of values reported is minimum and maxi..