Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.85 GPa | 994 ksi | STN EN ISO 178 |
Plastcom PLASTAMID® 6 GF 30 005 PA6 reinforced with glass fiber PA 6 for injection molding, reinforced with 30% glass fiber, used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools, gears, covers.. |
|||
Flexural Modulus | 6.85 GPa | 994 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 2200F PEI 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Flexural Modulus | 6.85 GPa | 994 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU2110 PEI 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Flexural Modulus | 6.85 GPa | 994 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU2200 PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Flexural Modulus | 6.85 GPa | 994 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp LFZ42XXC PEEK LNP THERMOCOMP* LFZ42XXC is a compound based on Polyetheretherketone resin containing Glass Fiber, Milled Glass. Added features of this material include: Low Warpage.This data was supplied by SABIC.. |
|||
Flexural Modulus | 6.85 GPa | 994 ksi | ASTM D790 |
PlastxWorld CEVIAN®-N GRSJ 20% GF SAN resin Glass fiber reinforced SAN resin. These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Modulus | 6.85 GPa | 994 ksi | ISO Data |
BASF Ultramid® 7523-2AM BK ND3007 33% Glass Filled PA66 (Conditioned) Ultramid 7523-2AM BK ND3007 is an impact modified, 33% glass reinforced, heat stabilized injection molding PA6/6. |
|||
Flexural Modulus | 6.85 GPa | 994 ksi | ASTM D790 |
BLUESTAR 101G20 PBT, 20% Glass Filled Typical Applications: Appliances, molded partsInformation provided by Polymer Technology and Services, LLC (PTS). |