Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.698 GPa | 971.5 ksi | ISO 178 |
Azdel Plus C507-B01 50% Chopped Fiber Mat / PP Resin Matrix (Mineral filled) AZDEL® C507-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat and mineral filler contained within a polypropylene resin matrix. This composite material featu.. |