Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.20528 - 8.27371 GPa @Temperature 150 - 150 °C |
900.014 - 1200.02 ksi @Temperature 302 - 302 °F |
Average value: 9.03 GPa Grade Count:1 |
Overview of materials for Vinyl Ester Sheet Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value.. |
|||
Flexural Modulus | 6.20528 - 8.27371 GPa @Thickness 0.500 - 2.50 mm |
900.014 - 1200.02 ksi @Thickness 0.0197 - 0.0984 in |
Average value: 9.03 GPa Grade Count:1 |
Overview of materials for Vinyl Ester Sheet Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value.. |
|||
Flexural Modulus | 6.20528 - 14.9616 GPa @Temperature -40.0 - 204 °C |
900.014 - 2170.03 ksi @Temperature -40.0 - 400 °F |
Average value: 9.58 GPa Grade Count:2 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |