Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.621 GPa | 90.0 ksi | Tangent; ASTM D790 |
RheTech Products FT1001-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Facias, claddings, and rocker panelsBodyside moldingsStep pads and bumper componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | Tangent; ASTM D790 |
RheTech Products FT1001-177UV Thermoplastic Polyolefin, Non-UV Stabilized, HS5 Medium Dark Neutral Applications: Scuff platesBodyside moldingsStep and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | Tangent; ASTM D790 |
RheTech Products FT2500-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | Tangent; ASTM D790 |
RheTech Products FT2500-594UV Thermoplastic Polyolefin, UV Stabilized, 9428NM Spectra Grey Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | Tangent; ASTM D790 |
RheTech Products FT2500-630UV Thermoplastic Polyolefin, UV Stabilized, 500F Light Charcoal Applications: Air DamsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | Tangent; ASTM D790 |
RheTech Products UVFT2500-01 Thermoplastic Polyolefin, 90K Flexural Modulus, UV Stabilized, Black Applications: Air damsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.621 - 0.827 GPa | 90.0 - 120 ksi | ASTM D790 |
Arkema Group Kynar Flex® 2900 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Flexural Modulus | 0.621 - 0.827 GPa | 90.0 - 120 ksi | ASTM D790 |
Arkema Group Kynar Flex® 3120 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Flexural Modulus | 0.621 - 8.27 GPa | 90.0 - 1200 ksi | Average value: 3.90 GPa Grade Count:47 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | ASTM D 790 |
Shakespeare Isocorâ„¢ 653 Nylon 6 Terpolymer Isocorâ„¢ 653 multi-polymer is a linear polyamide with unique solubility characteristics and physical properties. Isocorâ„¢ 653 is easily processed and has a wide range of applications due .. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | ASTM D790 |
Techmer ES HiFill FR® PP CO FR-N V2 Availability: North AmericaForms: PelletsFeatures: Flame Retardant, High Impact Resistance and CopolymerInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | ASTM D790 |
ScanTube PTFE Tubing Information provided by ScanTube, Inc. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | At 2 mm/min; ASTM D790 |
Borealis Borecene™ RM8402 Linear Polyethylene for Rotational Molding Borecene RM8402 is a third generation linear medium density natural polyethylene for rotational molding. The narrow molecular weight distribution imparted through metallocene catalyst technology pro.. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | At 2 mm/min; ASTM D790 |
Borealis Borecene™ RM8403 Linear Polyethylene for Rotational Molding Borecene RM8403 is a third generation linear medium density natural polyethylene for rotational molding. The narrow molecular weight distribution imparted through metallocene catalyst technology pro.. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | ASTM D790 |
Teknor Apex Telcar® TL-150 BLK288 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Speci.. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | ASTM D790 |
Teknor Apex Telcar® TL-150 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Speci.. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | ASTM D790 |
Chase Plastics CP Pryme® N100STL (COND, 50% RH) Nylon 6, Super Toughened, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | ASTM D790 |
Chase Plastics CP Pryme® N300STL (COND, 50% RH) Nylon 6 (Utility Grade), Super Toughened, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN100STL (COND, 50% RH) Nylon 66, Super Toughened, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN200STL (COND, 50% RH) Nylon 66, Super-Toughened, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | ASTM D3350 |
Chevron Phillips Marlex® HHM TR-418Q MDPE Hexene Copolymer High performance MDPE resin has been formulated for the demanding requirements of pressure pipe applications. Meets ASTM D4976 PE 225. Meets FDA Regulation 177.1520, suitable for food packaging ap.. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | ASTM D790 |
Ensinger HYDLAR® Z Nylon, Pultruded Aramid Fiber Reinforced (PA) HYDLAR® possesses a combination of physical properties that cannot be found in any other commercially available engineered plastic. Design engineers have created a family of superior wear and abra.. |
|||
Flexural Modulus | 0.621 - 1.65 GPa | 90.0 - 240 ksi | Average value: 0.990 GPa Grade Count:88 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |
|||
Flexural Modulus | 0.621 - 7.24 GPa | 90.0 - 1050 ksi | Average value: 1.79 GPa Grade Count:199 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
Flexural Modulus | 0.621 GPa | 90.0 ksi | ASTM D3350 |
Formosa Plastics Formolene® HP3902 Pipe HDPE Natural Medium Density Hexene CopolymerApplications: Pipe for gas distribution, oilfield and other industrial pipe, telecommunications conduit.Formolene HP3902 is a high performance copolymer that i.. |