Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0676 GPa | 9.80 ksi | at 10 pcf expanded density |
NOVA Chemicals Dylite® F271T Specialty Expandable Polystyrene Features: Highly consistent bead size; high gloss characteristics; low energy consumption; fast cyclingApplications: Drinking cups -hot and cold, noodle bowls, take-out and ice cream containers, and.. |
|||
Flexural Modulus | 0.0676 GPa | 9.80 ksi | Density 10 pcf |
NOVA Chemicals Dylite® F271TN Expandable Polystyrene Resin Highly consistent bead size, High gloss characteristics, Low energy consumption, Fast molding cycles, Food contact compliantApplications: Drinking cups (hot and cold), Noodle bowls, Take-out contai.. |
|||
Flexural Modulus | 0.0676 GPa | 9.80 ksi | Density 10 pcf |
NOVA Chemicals Dylite® F271TS Expandable Polystyrene Resin Highly consistent bead size, High gloss characteristics, Low energy consumption, Fast molding cycles, Food contact compliantApplications: Drinking cups (hot and cold), Noodle bowls, Take-out contai.. |