Mechanical Properties Metric English Comments
Flexural Modulus 6.15 GPa
892 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® CM6220 PC (Asia Pacific)
CYCOLOY CM6220 resin is a mineral filled grade featuring of high modulus (6GPa), good flow and ductility, low warpage. It is of non-Br & non-Cl flame retardant systems intended to meet thin wall fla..
Flexural Modulus 6.15 GPa
892 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® BM5225X PC (Asia Pacific)
BM5225X resin is a mineral filled grade featuring of high modulus, good flow and ductility, low warpage. It is of non-Br & non-Cl flame retardant systems intended to meet thin wall flame resistance ..
Flexural Modulus 6.15 GPa
892 ksi
Plastcom SLOVAMID 6 NG GF 20 HLS PA6, 20% glass fibre, combined stability
FeaturesPA 6 for injection moulding, chemically reinforced with 20% glass fibre, heat stabilized and weather stabilized. Stabilized against hydrolysis. Good surface finisch.Packaging, transport, sto..
Flexural Modulus 6.15 GPa
892 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP AF004AH ABS
LNP THERMOCOMP* AF004AH is a compound based on ABS resin containing 20% Glass Fiber. Added feature of this material is: Healthcare.
Flexural Modulus 6.15 GPa
892 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP AF004 ABS
LNP* THERMOCOMP* AF004 is a compound based on ABS resin containing 20% Glass Fiber.
Flexural Modulus 6.15 GPa
892 ksi
2 mm/min; ISO 178
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded
PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol..
Flexural Modulus 6.15 GPa
892 ksi
ISO 178
Azdel Plus R401-B01 40% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R401-B01 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a polypropylene resin matrix. This composite material features high flow pr..