Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.14 GPa | 890 ksi | ASTM D790 |
Polymer Resources PEI-G20 Polyetherimide, 20% Glass Reinforced Polyetherimide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Flexural Modulus | 6.14 GPa | 890 ksi | ASTM D790 |
Techmer ES Electrablend® ABS CF10 A1 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 6.14 GPa | 890 ksi | ASTM D790 |
Polymer Resources PEI-G20 Polyetherimide, 20% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |