Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1033STHL Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | tangent; ASTM D790 |
Spartech PP5930 Glass/Mica Reinforced Homopolymer Information provided by Spartech |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF20 HS L BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF20 L 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF20 SL4 HS BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer, Silicone Lubricant (4%) and LubricantFeatures: Heat Stabilize.. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Techmer ES HiFill® PP GF/M40 CC BK 40% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Techmer ES Plastiblend® TPX-HTN-000AB 15% Glass Filled Availability: North AmericaForms: Pellets Filler/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Techmer ES Statiblend® PA6/6 GF20 AS BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Lubricant, Antistatic and Heat StabilizerFeatures: Antistatic, Heat Stabilized and Lubricate.. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN113L (Dry) Nylon 66, 13% Glass Fiber Reinforced, Lubricated Features: Good chemical resistanceGrease resistantLubricatedOil resistantHigh rigiditySolvent resistantHigh tensile strengthForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
Clariant PA213M40BK Nylon 6, 40% Mineral Reinforced, Heat Stabilized, Black Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 5.52 - 16.0 GPa | 800 - 2320 ksi | Average value: 9.57 GPa Grade Count:34 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Flexural Modulus | 5.52 GPa | 800 ksi | ASTM D790 |
PolyOne Edgetek® SF-10GF/000 Polyphenylene Sulfide (PPS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |