Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.30 GPa | 769 ksi | |
Plastcom SLOVALEN PH 49 GF 30 TS PP, 30% glass fibre, mod. of mech. Properties FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | STN EN ISO 178 |
Plastcom SLOVALEN PH 61 GF 30 Polypropylene Homopolymer, 30% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fiber, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suit.. |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | STN EN ISO 178 |
Plastcom SLOVAMID 66 T 30 Polyamide 66, 30% Mineral Filled FeaturesPA 66 with the content of 30% chemically modified mineral filler. Used for holders of electric hand tools, hobby tools, gears, covers of electric tools, flat products, automobile wheel cove.. |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | STN EN ISO 178 |
Plastcom SLOVAMID® 6 GF 25 E LS PA6 reinforced with glass fiber, UV stabilized PA 6 grade for extrusion, reinforced with 25% glass fiber, determined for extrusion of window profile systems. Delivered in natural as well as full RAL scale color.Information Provided by Plastcom s.. |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | STN EN ISO 178 |
Plastcom SLOVASTER® B1 GF 15 FRL 4 PBT reinforced with glass fibers, flame retarded PBT reinforced with 15 % glass fiber, flame retarded with the halogen flame retardant. Anisotropy of shrinkage enables the injection molding of round, cylindrical or other hole products. Application.. |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | ISO 178 |
Nilit FRIANYL A63 W-GV20 Nylon 6.6 for injection molding, 20% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP FARADEX NX07344 PC+ABS (Asia Pacific) Faradex NX07344 is a compound based on PC+ABS blend resin containing non-brominated and non-chlorinated flame retardant system, Stainless Steel and glass fiber. Added features of this material incl.. |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL34 PC (Europe-Africa-Middle East) LNP* Lubricomp* DFL34 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® C4220 PC+ABS (Europe-Africa-Middle East) CYCOLOY C4220 is a 20% glass reinforced, non FR PC+ABS grade. It shows high heat resistance, excellent strength and rigidity with good cosmetic appearance that combines a good processabity with a lo.. |
|||
Flexural Modulus | 5.30 GPa @Temperature 23.0 °C |
769 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPH GF8030 PD1 VT2 PP, Glass Fiber-Reinforced, Chemically Coupled Heat Stabilized Information provided by Polykemi AB |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | ISO 178 |
Lanxess Durethan® AKV 15 H3.0 000000 Nylon 66, 15% Glass Fibers PA 66, 15% glass fibers, injection molding, heat-ageing stabilized |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | ISO 178 |
Solvay Technyl® A216V15 15% Glass Filled Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NF1520 PPE+PS LNP* Lubricomp* Noryl_NF1520 compound is a 20% glass reinforced, 15% PTFE. Wear resistant; 211F HDT @ 264 psi. |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | ISO 178 |
Solvay TECHNYL® eXten D238 V30 Nylon 6,10, 30% glass fiber, Conditioned Description: TECHNYL® eXten D 238 V30 is a PA6,10 30% glass fiber reinforced and impact modified suitable for injection molding. TECHNYL® eXten D 238 V30 is based on a partially bio-sourced po.. |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON RFD03 PA 66 (Asia Pacific) LNP* STATKON* RFD03 is a compound based on PA 66 resin contaning Carbon Powder, Glass Fiber. Added features include: Electrically Conductive. |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp CF004 PS (Europe-Africa-Middle East) LNP* Thermocomp* CF004 is a compound based on Polystyrene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp IFB33 PA 6/12 LNP* Thermocomp* IFB33 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp IFB33 PA 6/12 (Asia Pacific) LNP* Thermocomp* IFB33 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp MX88073 PP (Asia Pacific) LNP* Thermocomp* MX88073 is a compound based on Polypropylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PX138H PPE+HIPS (Asia Pacific) Modified PPO Resin with 20% Glass Fibre Reinforced |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® SHF4930 PBT (Europe-Africa-Middle East) Super high flow FR PBT grade with 15% Glass reinforced |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RFZ22S PA 66 LNP* THERMOCOMP* RFZ22S is a compound based on Nylon 66 resin containing 10% Glass Fiber, 10% Milled Glass. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color .. |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. Noryl GFN1520V cust spec 1977 has been certified for potable water applications up to 85C in Europe and No.. |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | DAM; ISO 178 |
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66 Minlon 11C40 BKB086 is a 40% mineral reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers.. |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam PX05004 PA66, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX05004 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | ASTM D790 |
Ashley Polymers Ashlene® 827L-25G Nylon 6, 25% Glass Reinforced A 25% glass reinforced high impact Nylon 6 designed for applications requiring a high level of toughness, as well as superior low temperature properties.Data provided by the manufacturer |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | ISO Data |
BASF Ultramid® B3EG3 BK00564 15% Glass Filled PA6 (Dry) Ultramid B3EG3 BK00564 is a 15% glass fiber reinforced, pigmented black injection molding PA6 grade for housings with enhanced impact resistance. |
|||
Flexural Modulus | 5.30 GPa | 769 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® V9235 PET (Europe-Africa-Middle East) Valox heat stabilized, 15% Glass filled grade with mold release based on recycle PET. This grade is typically applied for business Machines applicationsThis data was supplied by SABIC-IP for the Eu.. |