Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.520 GPa | 75.4 ksi | ASTM D790 |
Nylene® PA6 Impact Modified 323 HS Nylon 6 Extrusion Grade; Dry as molded.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Flexural Modulus | 0.520 GPa | 75.4 ksi | ASTM D790 |
NOVA Chemicals Sclair® 2316 LLDPE Injection Molding Resin Features: Low odor, low warpage, fast cycling, high surface gloss, permits light weight lid design.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.520 GPa | 75.4 ksi | 1% Strain Value from rotomolded samples; ASTM D790 |
NOVA Chemicals Sclair® 8107 UV8D Butene LLDPE Rotational Molding Resin Excellent ESCR, Excellent low temperature impact properties, Excellent low shrinkage and warpage properties, Very good processability, UL 94-HB listedApplications: Food and laundry materials handlin.. |
|||
Flexural Modulus | 0.520 GPa | 75.4 ksi | ASTM D790 |
NOVA Chemicals Sclair® 2315 LLDPE Injection Molding Resin
(discontinued **) Features: Low odor, low warpage, fast cycling, high surface gloss, permits light weight lid design, low temperature impact excellent.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.520 GPa | 75.4 ksi | ASTM D790 |
NOVA Chemicals Sclair® 2318 LLDPE Injection Molding Resin
(discontinued **) Features: Low odor, low warpage, fast cycling, high surface gloss, permits light weight lid design.Applications: Thin walled container lids and closures.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.520 GPa | 75.4 ksi | 1% Strain Value from rotomolded samples; ASTM D790 |
NOVA Chemicals Sclair® 8107G UV8D Butene LLDPE Rotational Molding Resin Excellent ESCR, Excellent low temperature impact properties, Excellent low shrinkage and warpage properties, Very good processability, UL 94-HB listedApplications: Food and laundry materials handlin.. |
|||
Flexural Modulus | 0.520 GPa | 75.4 ksi | ASTM D790 |
NOVA Chemicals Sclair® 8306 UV8D, 8306G UV8D MDPE Rotational Molding Resin
(discontinued **) Features: Balanced combination of toughness, ESCR and processability.Applications: General purpose.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.520 - 1.30 GPa | 75.4 - 189 ksi | Average value: 0.850 GPa Grade Count:5 |
Overview of materials for Nylon 612, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Impact Modified". Each property range of values reported is minimum and maximum values of app.. |
|||
Flexural Modulus | 0.520 GPa | 75.4 ksi | ASTM D790 |
UBE P7115U Electronic Grade Nylon Copolymer Powder Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Flexural Modulus | 0.520 GPa | 75.4 ksi | ASTM D790 |
UBE 7115U Nylon 6/12 Copolymer Description: UBESTA Nylon 12 CopolymerInformation provided by UBE. |
|||
Flexural Modulus | 0.520 GPa | 75.4 ksi | ASTM D790 |
Ashley Polymers Ashlene® 734LD Nylon 6 A plasticized, highly flexible Nylon 6 with high impact resistance.Data provided by the manufacturer |
|||
Flexural Modulus | 0.520 - 13.8 GPa | 75.4 - 2000 ksi | Average value: 2.82 GPa Grade Count:27 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Flexural Modulus | 0.520 GPa | 75.4 ksi | ISO 178 |
Lubrizol ESTALOC® 59003 Ester-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |