Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.03 GPa | 730 ksi | ASTM D790 |
PolyOne Maxxam™ PPR-30G Black Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Modulus | 5.03 GPa | 730 ksi | ASTM D790 |
PolyOne Maxxam™ PPR-30G Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Modulus | 5.03 GPa | 730 ksi | ASTM D790 |
PolyOne Maxxam™ X MX5210-0030 RS Natural Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Modulus | 5.03 GPa | 730 ksi | ASTM D790 |
Polymer Resources TP-FRHG15 Polybutylene Terephthalate, 15% Glass Reinforced Alloy, Flame Retardant Polybutylene Terephthalate, 15% Glass Reinforced Alloy, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Flexural Modulus | 5.03 GPa | 730 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6 GF15 IM HS L 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Flexural Modulus | 5.03 GPa | 730 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6 GF18 IM 511 18% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 18% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Flexural Modulus | 5.03 GPa | 730 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM AR9100 PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Flexural Modulus | 5.03 GPa | 730 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® DR48 PBT 17% glass reinforced, flame retardant grade UL-94 rated V-0/5VA. |
|||
Flexural Modulus | 5.03 GPa | 730 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® DR48 PBT (Asia Pacific) 17% glass reinforced, flame retardant grade UL-94 rated V-0/5VA. |
|||
Flexural Modulus | 5.03 GPa | 730 ksi | ASTM D790 |
Techmer ES HiFill® PA4/6 M/GF 20 HS 20% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 50% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 5.03 GPa | 730 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF/M30 HS BK 10/20% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight and Mineral, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat .. |
|||
Flexural Modulus | 5.03 GPa | 730 ksi | ASTM D790 |
Star Plastics ABSGF20 Molding Grade ABS With 20% Glass Information provided by Star Plastics, Inc. |
|||
Flexural Modulus | 5.03 GPa | 730 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOTUF PX95726 PA 6 LNP THERMOTUF* PX95726 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 5.03 GPa | 730 ksi | ASTM D790 |
Chase Plastics CP Pryme® N333GL (COND, 50% RH) Nylon 6 (Utility Grade), 33% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 5.03 GPa | 730 ksi | ASTM D790 |
Ensinger Tecapeek® XP-96BHT Compression Molded PEEK HT, Unfilled, Black Pigmented Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Flexural Modulus | 5.03 GPa | 730 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-30FG-0600R 30% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 5.03 GPa | 730 ksi | ISO Data |
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Conditioned) Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a
balance of st.. |
|||
Flexural Modulus | 5.03 GPa | 730 ksi | ISO Data |
BASF Ultramid® 8333G HI HS BK-102 33% Glass Filled PA6 (Conditioned) Ultramid 8333G HI HS BK-102 is a 33% glass reinforced, heat stabilized, impact modified, pigmented black, PA6 injection molding compound developed for applications requiring improved dry as molded t.. |
|||
Flexural Modulus | 5.03 GPa | 730 ksi | ASTM D790 |
Asahi Kasei Thermylene® P-30FG-0812 30% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 5.03 GPa | 730 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-30FG-0600 30% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 5.03 GPa | 730 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-30FG-1804 30% Glass Fiber Reinforced, Heat and UV Information provided by Asahi Thermofil |
|||
Flexural Modulus | 5.03 GPa | 730 ksi | ASTM D790 |
Chase Plastics CP Pryme® N233GL (COND, 50% RH) Nylon 6, 33% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 5.03 GPa | 730 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGN2000A PC (Europe-Africa-Middle East) LNP* Thermocomp* Lexan_LGN2000A compound is a 20% glass reinforced PC, high flow. UL rated V-0. Consumer Electronics applications. |
|||
Flexural Modulus | 5.03 GPa | 730 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM AR9100 PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |