Polymer Property : Flexural Modulus = 712 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.91 GPa
712 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DFL34 PC
LNP LUBRICOMP* DFL34 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 4.91 GPa
712 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DFL34H PC
LNP LUBRICOMP* DFL34H is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Healthcare.