Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.490 GPa | 71.0 ksi | At 2 mm/min; ASTM D790 |
Borealis Borecene™ RM8342 Linear Polyethylene for Rotational Molding Borecene RM8342 is a third generation linear medium density natural polyethylene for rotational molding. The narrow molecular weight distribution imparted through metallocene catalyst technology pro.. |
|||
Flexural Modulus | 0.490 GPa | 71.0 ksi | At 2 mm/min; ASTM D790 |
Borealis Borecene™ RM8342RC Linear Polyethylene for Rotational Molding Borecene RM8342RC is a third generation linear medium density natural polyethylene for rotational molding. Borecene RM8342RC is a special grade, which has passed many rigorous tests and can be cons.. |
|||
Flexural Modulus | 0.490 GPa | 71.0 ksi | At 2 mm/min; ASTM D790 |
Borealis Borecene™ RM8343 Linear Polyethylene for Rotational Molding Borecene RM8343 is a third generation linear medium density natural polyethylene for rotational molding. The narrow molecular weight distribution imparted through metallocene catalyst technology pro.. |
|||
Flexural Modulus | 0.490 GPa | 71.0 ksi | At 2 mm/min; ASTM D790 |
Borealis Borecene™ RM8343RC Linear Polyethylene for Rotational Molding Borecene RM8343RC is a third generation linear medium density natural polyethylene for rotational molding. Borecene RM8343RC is a special grade, which has passed many rigorous tests and can be cons.. |
|||
Flexural Modulus | 0.490 - 0.892 GPa | 71.0 - 129 ksi | Average value: 0.632 GPa Grade Count:33 |
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Rotational Molded". Each property range of values reported is minimu.. |