Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0520 GPa | 7.54 ksi | method 1, Proc.B; ASTM D-790 |
Multibase Multi-Flex® TPE A 8502 LC BLK Multi-Flex® LC compounds are a new generation elastomers exhibiting improved compression set at elevated temperature. Multi-Flex® TPE compounds are based on Shell's Kraton G technology and featur.. |
|||
Flexural Modulus | 0.0520 GPa | 7.54 ksi | ASTM D790 |
A. Schulman POLYFORT™ PX 1042 Information provided by A. Schulman. |
|||
Flexural Modulus | 0.0520 GPa | 7.54 ksi | ASTM D790 |
A. Schulman POLYFORT™ PX 1042 Information provided by A. Schulman. |
|||
Flexural Modulus | 0.0520 GPa | 7.54 ksi | ASTM D790 |
A. Schulman POLYFORT™ PX 1042 Information provided by A. Schulman. |
|||
Flexural Modulus | 0.0520 GPa | 7.54 ksi | ASTM D790 |
A. Schulman POLYFORT™ PX 1042 Information provided by A. Schulman. |
|||
Flexural Modulus | 0.0520 GPa | 7.54 ksi | ASTM D790 |
DuPont Elvax® 550 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Flexural Modulus | 0.0520 GPa | 7.54 ksi | ASTM D790 |
A. Schulman POLYFORT™ PX 1042 Information provided by A. Schulman. |
|||
Flexural Modulus | 0.0520 GPa | 7.54 ksi | ASTM D790 |
A. Schulman POLYFORT™ PX 1042 Information provided by A. Schulman. |
|||
Flexural Modulus | 0.0520 GPa | 7.54 ksi | 1% Secant, ASTM D790 |
ExxonMobil Escorene® LD-730 High EVA Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Applications: Injection molding; Foams.. |