Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.79 GPa | 695 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOTUF PX95726 PA 6 LNP THERMOTUF* PX95726 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |