Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.71 GPa @Thickness 3.20 mm |
683 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID GP2130A(W) PA6+GF13%, General Purpose Feature: Injection Molding, PA6+GF13%, General PurposeApplication: Automotive PartsCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Modulus | 4.71 GPa | 683 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® EH7020HF PBT+PET Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developed for automotive bezel application that requires basecoat + .. |
|||
Flexural Modulus | 4.71 GPa | 683 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® EH7020HF PBT+PET (Asia Pacific) Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developped for automotiove bezel application that require basecoat +.. |
|||
Flexural Modulus | 4.71 GPa | 683 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp GF003 PSU LNP THERMOCOMP* GF003 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 4.71 GPa | 683 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp ZZ006 PPE+PS LNP THERMOCOMP* ZZ006 is a compound based on PPE+PS Blend resin containing Milled Glass.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 4.71 GPa | 683 ksi | ISO 178 |
Polyplastics Duranex® 3116 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 7.5% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 4.71 GPa | 683 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOTUF WF003I Polyester, TP LNP THERMOTUF* WF003I is a compound based on Polyester, TP resin containing Glass Fiber. Added features of this material include: High Impact. |