Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.70 GPa | 682 ksi | |
Plastcom SLOVALEN PC 59 GF 30 PP, 30% glass fibre FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains themodifier of mechanical properties.Increased strength in comparison with unfilled PP. A.. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | |
Plastcom SLOVAMID 66 GF 15 T 6 TS PA66, 15% glass fibre, 6% talc FeaturesChemically reinforced with 15% glass fibre and 6% of talc, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrica.. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | |
Plastcom SLOVAMID 66 GF 20 HI PA66, 20% glass beads FeaturesChemically reinforced with 20% glass beeds, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. I.. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | ISO 178 |
Nilit FRIANYL A63 SG-GV 2010 Nylon 6.6 for injection molding, 20% mineral filled and 10% glass fiber reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 4.70 GPa @Temperature 23.0 °C |
682 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Crastin® HR5315HF BK503 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |
|||
Flexural Modulus | 4.70 GPa @Temperature 90.0 °C |
682 ksi @Temperature 194 °F |
ASTM D790 |
LATI LARIL 13-V1KC Mineral Filled Polyphenylene Oxide (PPOm) (UL94V-1)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | ISO 178 |
Nilit FRIANYL A63 KV40 Nylon 6.6 for injection molding, 40% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | ISO 178 |
Nilit FRIANYL B63 H-GV15 Nylon 6 for injection molding, 15% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | <= 4.70 GPa | <= 682 ksi | |
Reliance Industries Polypropylene - Talc filled Information provided by Reliance Industries |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | ASTM D790 |
IRPC Polimaxx Polene 2311LCX GA4 Polypropylene Compound CHARACTERISTICS: POLYPROPYLENE BLOCK COPOLYMER WITH 20% GLASS FIBRE REINFORCED, HIGH IMPACT STRENGTH, HIGH MECHANICAL STRENGTH, HIGH STIFFNESS, LOW SHRINKAGEAPPLICATIONS: INJECTION MOLDING FOR AUTOP.. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 130 H2.0 DUS008 901510 Nylon 6, Glass Fiber Reinforced, Impact Modified PA 6, 30% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | ISO 178 |
Solvay TECHNYL® B 218 V30 Black 21 N PA66, 30% glass fiber, Conditioned Description: Copolyamide PA66/6, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 218 V30 is used i.. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | ISO 178 |
Solvay TECHNYL® B 218L V30 Black 44 N PA66, 30% glass fiber, Conditioned Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistance.Available in: Asia Pacific, Europe and Latin AmericaProdu.. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MX06402H PP LNP* THERMOCOMP* MX06402H is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Heat Stabilized, Low Extractable. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® 815F PBT+PET (Asia Pacific) PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® SHF4930 PBT Super high flow FR PBT grade with 15% Glass reinforced |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MC002 PP LNP* THERMOCOMP* MC002 is a compound based on Polypropylene resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp PFB42ES PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PFB42ES is a compound based on PA6 resin containing Glass Fiber, Glass Bead. Added features include: Easy Molding, Heat Stabilized.This data was supplied by SABIC-IP for the Europe-.. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | ISO 178 |
Solvay TECHNYL® A 216 S40 PA66, 40% glass spheres, DRY Description: Polyamide 66, reinforced with 40% of glass spheres, for injection molding.Available in: EuropeProduct Applications: TECHNYL ® A 216 S40 is used in all sectors of industry, offering a.. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | ISO 178-93 |
Wellman Wellamid® MR340 42H-NBK1 Nylon 6, 34% Mineral Reinforced All information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide PFB42EU PA6, Glass Fiber/Bead Filled, Injection Molded Starflam PFB42EU is an UV Stabilized, Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide PX05046 PA6, Glass Bead/Fiber Filled, Injection Molded Staramide XP05046 is Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | ISO 178 |
BASF Ultramid® B3ZG6 BK 30564 30% Glass Filled PA6-1 (Conditioned) Description: Impact-modified and 30% glass fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas.. |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | Wet; ASTM D790 |
Asahi Kasei Leona® 13G25 25% Glass Filled Nylon 66 Enhanced strength, stiffness and durability; with 25% GF.Applications:Automotive parts Information provided by Asahi Kasei |
|||
Flexural Modulus | 4.70 GPa @Temperature 23.0 °C |
682 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYabs F20 GF17 ABS, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 4.70 GPa @Temperature 120 °C |
682 ksi @Temperature 248 °F |
ISO 178 |
DSM Stanyl® TS200F6 PA46-GF30 30% Glass Reinforced |
|||
Flexural Modulus | 4.70 GPa | 682 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp PFB42EU PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PFB42EU is a compound based on PA 6 resin containing Glass Fiber, Glass Bead. Added features include Easy Molding, Heat Stabilized.This data was supplied by SABIC-IP for the Europe-.. |