Polymer Property : Flexural Modulus = 63.5 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.438 GPa
63.5 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE D 5303 BLK
Ash is 2%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Flexural Modulus 0.438 GPa
63.5 ksi
Dow DOWLEX™ 2503.10 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2503.10 Polyethylene resin is a narrow molecular weight distribution copolymer designed as a superior processing resin. For very thin wall higher cavitation molding, this grade often is a p..