Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 62.00 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.4275 GPa
62.00 ksi
ASTM D790
DuPont™ Surlyn® 9120 Ionomer Resin, Zinc
Surlyn® 9120 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr..
Flexural Modulus 0.4275 GPa
62.00 ksi
2% secant; ASTM D790
ExxonMobil LL 6100.17 Injection Molding Resin
Product Description: LL 6100 is a narrow molecular weight butane copolymer designed for applications that require easy processability. This resin offers outstanding toughness and tear resistance in ..