Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Quadrant EPP Duratron® PAI T4203 Extruded Polyamide-imide (ASTM Product Data Sheet) |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Polymer Resources PC/TP-GP3-G20 PC/Polyester Alloy, 20% Glass Reinforced Superior Chemical Resistance, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
PolyOne Edgetek® NL-08GF-02CF/000 Nylon 6/12, Glass/Carbon Fiber Filled
(discontinued **) Description/Features:Glass/Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | Flexural 0.5% Secant Modulus; ASTM D790 |
Greene Tweed Arlon® 1000 Polyketone Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Techmer ES HiFill® HDPE GF30 UV 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Good UV ResistanceAdditive: UV StabilizerInformation provided by TP Composites.. |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 CM25 HS BK 25% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 25% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackInformation provided by TP Compo.. |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Techmer ES HiFill® PES GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Techmer ES HiFill® PSU GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific) LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Clariant 6004G13-HSL BK UV Black Nylon 6, 13% Glass Fiber Reinforced Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Clariant 6004G8-HSL BK UV Black Nylon 6, 8% Glass Fiber Reinforced Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
PolyOne Edgetek® ES-10GF/000 PES (Polyethersulfone), 10% Glass Reinforced, Hi-Temp
(discontinued **) Information provided by PolyOne™ Corporation |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | secant; ASTM D790 |
Spartech EP6430 Filled and Reinforced Copolymer Filled copolymers offer a higher level of impact performance than homopolymer materials, and higher stiffness than unfilled copolymers. Copolymer based materials retain much of their impact strength.. |